Re-activation of Chrome

Q. Do you have an easy way of re-activating a hard chrome plated surface? This would be so that more hard chrome can be added.

A. Solvent clean or Degrease (as required), warm up in heated chrome bath with for 2-10 minutes with current off, calculate warm up time based on part temperature, size and girth. Reverse etch in the chrome bath for 30 seconds to 1 minute at approximately 5 - 6 volts DC. Then switch to forward polarity and step the DC voltage up incrementally from 2.0- volts to full amps, approximately .2 of a volt per step, at 15 second intervals until desired plating range is reached. Then calculate thickness required and set re-plating time.

Good luck.

Randy Taylor

 

 

 

 


The information contained in this site is provided for your review and convenience. It is not intended to provide legal advice with respect to any federal, state, or local regulation.
You should consult with legal counsel and appropriate authorities before interpreting any regulations or undertaking any specific course of action.

Please note that many of the regulatory discussions on STERC refer to federal regulations. In many cases, states or local governments have promulgated relevant rules and standards
that are different and/or more stringent than the federal regulations. Therefore, to assure full compliance, you should investigate and comply with all applicable federal, state and local regulations.